1. Overlapping angle

In the process of production, color film, the matte sheet must be smoothed

2. Pit

Clean up the dirt on the embossed plate in time.

3. Black dot

Develop good operating habits, don't bring dirt between printing and matte

4. Matte film wrinkle

Renew the matte film in time

5. Crease on the back of the embossed plate

Take care of the embossed version used, and find the damage in time to reflect and replace.

6. Glass fiber dirty.

Clean up in time, don't bring glass fiber into the color film.

7. Indentation

Replace matt film in time.

8. Cracked film.

If there are holes in the film, replace them in time.

9. Discoloration.

Timely adjustment of production and production process.

10. Shading scar.

Take care of the shading plate, no foreign matter can stick on the surface; remove it if found; replace the shading plate in time.