Welcome!
  • 0086 13321818576 (Steven Lee)
News
Current Location:Home > News

What are the reasons for the PVC floor blistering

Update:2019/7/18 17:38:17 Views:15

In daily life, PVC flooring may appear to be foaming and curling. What is the cause of this phenomenon?

1. It is caused by improper construction process.

2. It is a problem with the material of the floor itself.

3. It may be that the adhesive is selected incorrectly.

pvc flooring

Some floors may be produced with less strict control and the floor size change rate is too large. Subject to thermal expansion and contraction. There is also that when the construction is not rolled, the glue misses the best opening time and loses the adhesion. The main problem after the sheet is laid is the warping.

The main problem of coiling is the blistering. When the whole floor is covered on the ground, the air is generated inside the paving. If it is not removed in time, it is difficult to repair.

resilient vinyl floor

In order to save the cost of accessories, some merchants use pressure-sensitive adhesive to directly stick to the coiled resilient vinyl floor. The consequences can be imagined. The foaming and curling is also common, so a good product and a reliable installation team with construction technology. The supporting construction materials can reduce the quality problems to a certain extent.

Therefore, when we choose the PVC plastic floor brand, we must choose the regular manufacturer & supplier in China, so that the product quality can be guaranteed.